2026 HCI + DHS H3 Prelim insert final
Uploaded by Kozak327 · 10 November 2026
Preview
Text from the first pagesThis document has 4 pages. Any blank pages are indicated. HWA CHONG INSTITUTION C2 Preliminary Examination Higher 3 CANDIDATE NAME CT GROUP 2 5 S H3 CLASS A / C / N CHEMISTRY Paper 1 INSERT 9813/01 22 September 2026 2 hour 30 minutes INFORMATION • This insert contains information for Question 1. • You may annotate this insert and use the blank spaces for planning. Do not write your answers on the insert. This paper is a collaboration between HCI and DHS.
2 © Hwa Chong Institution 2026 9813/01/C2 Preliminary Examination DO NOT WRITE IN THIS MARGIN DO NOT WRITE IN THIS MARGIN DO NOT WRITE IN THIS MARGIN DO NOT WRITE IN THIS MARGIN DO NOT WRITE IN THIS MARGIN [Turn Over Information for Question 1 Plastics pollution is causing an environmental crisis, prompting the development of new approaches to recycle and upcycle plastics. Innovations in plastics depolymerisation is critical to incentivise improved plastics recycling and upcycling, thereby reducing the severe global burden of plastic waste. Thermodynamics and kinetics of polymer depolymerisation In polymer synthesis, the ceiling temperature, Tc, of a polymer is the temperature at which the rate of depolymerisation equals the rate of polymerisation. Above Tc, it is thermodynamically favoured for polymers to depolymerise. Equation 1 shows the depolymerisation of a common polymer, polyethylene. equation 1 H H n n CH2=CH2 + 2H polyethylene Table 1.1 shows the ceiling temperatures of polyethylene and polyisobutylene. Table 1.1 polymer monomer Tc / °C polyethylene CH2=CH2 610 polyisobutylene CH2=C(CH3)2 175 However, thermodynamically favoured depolymerisation does not necessarily occur at appreciable rates. Emerging approaches to accelerate polymer depolymerisation have been developed. The following are two examples of such approaches. Microwave-assisted catalysis of polyethylene depolymerisation An effective microwave-assisted process for recycling low-density polyethylene (LDPE) waste was reported. After just 1 h of microwave irradiation at a frequency of 2.45 GHz at 180 °C in relatively dilute nitric acid solution, LDPE powder was totally degraded. This transformation led to a few well-defined water-soluble dicarboxylic acids as shown in Figure 1.1. polyethylene OH OH O O m m = 1, 2, ... or 5 microwave HNO3(aq) H H n Figure 1.1 The degradation product mixture of LDPE was treated with excess aqueous sodium hydroxide and then freeze-dried for analysis using infrared (IR) spectroscopy.
3 © Hwa Chong Institution 2026 9813/01/C2 Preliminary Examination DO NOT WRITE IN THIS MARGIN DO NOT WRITE IN THIS MARGIN DO NOT WRITE IN THIS MARGIN DO NOT WRITE IN THIS MARGIN DO NOT WRITE IN THIS MARGIN [Turn Over Hydrogenative depolymerisation of nylon-6 Figure 1.2 shows the hydrogenative depolymerisation of nylon-6 in the presence of a ruthenium catalyst at 150 °C and 70 bar H2. Nylon-6 and the catalyst were first dissolved in dimethyl sulfoxide (DMSO) and then the polymer was converted into its hydrogenated monomer, 6-amino-1-hexanol, as well as its dimer and trimer under the catalytic conditions. nnylon-6 H2, Ru catalyst N H O NH2 OH 6-amino-1-hexanol 150 oC + dimer + trimer Figure 1.2 The structures of DMSO and the ruthenium catalyst are shown in Figure 1.3. N N H CH3 P CH3 CH3 HRu catalyst CH3 S CH3 O DMSO Figure 1.3 The hydrogenative depolymerisation of nylon-6 involves the cleavage of its amide linkages. The 3-step process leading to the C−N bond dissociation is shown in Figure 1.4. N N H CH3 P CH3 CH3 Ru H H step 1H2 R N R O H R N R O H H H N R H R O + R OH step 2 step 3 catalyst activated catalyst R = alkyl groups Figure 1.4
4 © Hwa Chong Institution 2026 9813/01/C2 Preliminary Examination DO NOT WRITE IN THIS MARGIN DO NOT WRITE IN THIS MARGIN DO NOT WRITE IN THIS MARGIN DO NOT WRITE IN THIS MARGIN DO NOT WRITE IN THIS MARGIN [Turn Over BLANK PAGE
This document has 4 pages. Any blank pages are indicated.
Content continues in the PDF. Download PDF
